Polyester T100 Based Casting Polyurethane Prepolymer
video
Polyester T100 Based Casting Polyurethane Prepolymer

Polyester T100 Based Casting Polyurethane Prepolymer

Polyester based polyurethane prepolymer have superior cut, tear, abrasion, oil and solvent resistance.

  • 빠른 배송
  • 품질 보증
  • 연중무휴 고객 서비스
제품 소개

Polyester based polyurethane prepolymer have superior cut, tear, abrasion, oil and solvent resistance.


Item

Type

HJ-3170

HJ-3175

HJ-3180

HJ-3185

NCO percent Content

2.3±0.2

2.7±0.2

3.0±0.2

3.5±0.2

Density25 degree /(g/cm³)

1.23

1.23

1.23

1.23

Viscosity80 degree /mpa·s

2200-2500

1800-2100

1700-2000

1500-1800

Appearance at 25 degree

White solid

MixTemperature degree

Prepolymer /Moca

85 degree /115 degree

85 degree /115 degree

85 degree /115 degree

85 degree /115 degree

Gel Time /min

35-45

20-30

15-18

12-16

Vulcanization Time (h)

25-16

25-16

25-16

25-16

Physical Properties

Hardness (Shore A)

70±2

75±2

80±2

85±2

Tensile Strength (Mpa)

30-35

35-40

38-43

43-47

100 percent Modulus (Mpa)

8-10

8-10

8-10

9-10

300 percent Modulus (Mpa)

16-17

16-17

16-18

16-18

Elongation at Break ( percent )

600-650

620-680

650-700

650-720

Tear Strength (KN/m)

55-65

60-75

85-90

90-100

Compression permanent deformation percent

4-6

4-6

4-6

2-4

DIN Abrasion lossmm³

Less than or equal to 50

Less than or equal to 50

Less than or equal to 45

Less than or equal to 45

Resilience percent /25 degree

25-28

23-26

22-24

18-22

Product application : Roller, mining tire, classification screen, pipeline lining, coupling,, mining conveyor belt, printing scraper, industrial caster, pipeline cleaner, pump lining, flotation cell impeller and other products.

Operation details:

After vacuum degasing at 80-85 degree , the prepolymer is mixed with melted MOCA for casting and vulcanization. It is suitable for manual and mechanical operation.

Storage:

Store in a cool and dry place and use up as soon as possible after opening; If it cannot be used up at one time, it shall be sealed with nitrogen; The second opening needs to be used for defoaming, and the original storage period is six months.

packing:

20kg or 200kgiron drum


Item

Type

HJ-3135

HJ-3190

HJ-3190A

HJ-3190C

NCO percent Content

3.5±0.2

4.3±0.2

4.3±0.2

4.2±0.2

Density25 degree /(g/cm³)

1.23

1.23

1.23

1.23

Viscosity80 degree /mpa·s

1500-1800

1100-1400

1200-1500

1200-1500

Appearance at 25 degree

White solid

MixTemperature degree

Prepolymer /Moca

85 degree /115 degree

80 degree /115 degree

80 degree /115 degree

80 degree /115 degree

Gel Time /min

16-22

8-12

6-9

12-16

Vulcanization Time (h)

25-16

25-16

25-16

25-16

Physical Properties

Hardness (Shore A)

85±2

90±2

90±2

90±2

Tensile Strength (Mpa)

43-47

45-52

43-50

46-53

100 percent Modulus (Mpa)

8-10

8-10

8-10

8-10

300 percent Modulus (Mpa)

14-16

15-17

14-16

16-18

Elongation at Break ( percent )

600-750

580-700

600-710

550-650

Tear Strength (KN/m)

95-110

100-120

95-110

110-125

Compression permanent deformation percent

4-6

2-4

2-4

2-4

DIN Abrasion lossmm³

Less than or equal to 50

Less than or equal to 40

Less than or equal to 48

Less than or equal to 40

Resilience percent /25 degree

20-23

16-19

18-22

15-18

Product application : Roller, mining tire, classification screen, pipeline lining, coupling,, mining conveyor belt, printing scraper, industrial caster, pipeline cleaner, pump lining, flotation cell impeller and other products.

Operation details:

After vacuum degasing at 80-85 degree , the prepolymer is mixed with melted MOCA for casting and vulcanization. It is suitable for manual and mechanical operation.

Storage:

Store in a cool and dry place and use up as soon as possible after opening; If it cannot be used up at one time, it shall be sealed with nitrogen; The second opening needs to be used for defoaming, and the original storage period is six months.

packing:

20kg or 200kgiron drum


Item

Type

HJ-3193

HJ-3195

HJ-3195A

HJ-3197

NCO percent Content

4.7±0.2

5.0±0.2

5.5±0.2

6.5±0.2

Density25 degree /(g/cm³)

1.23

1.23

1.23

1.23

Viscosity80 degree /mpa·s

1000-1300

900-1200

900-1300

800-1100

Appearance at 25 degree

White solid

MixTemperature degree

Prepolymer /Moca

80 degree /115 degree

75 degree /115 degree

75 degree /115 degree

75 degree /115 degree

Gel Time /min

6-9

7-10

5-8

3-6

Vulcanization Time (h)

25-16

25-16

25-16

25-16

Physical Properties

Hardness (Shore A)

93±2

95±2

95±2

97±2

Tensile Strength (Mpa)

48-55

50-55

48-53

46-55

100 percent Modulus (Mpa)

8-10

9-10

9-10

9-10

300 percent Modulus (Mpa)

16-18

18-22

16-18

18-22

Elongation at Break ( percent )

450-600

400-550

530-700

400-550

Tear Strength (KN/m)

100-120

110-130

110-130

115-130

Compression permanent deformation percent

2-4

2-4

2-4

2-4

DIN Abrasion lossmm³

Less than or equal to 45

Less than or equal to 45

Less than or equal to 45

Less than or equal to 45

Resilience percent /25 degree

15-18

14-16

13-16

12-15

Product application : Roller, mining tire, classification screen, pipeline lining, coupling,, mining conveyor belt, printing scraper, industrial caster, pipeline cleaner, pump lining, flotation cell impeller and other products.

Operation details:

After vacuum degasing at 80-85 degree , the prepolymer is mixed with melted MOCA for casting and vulcanization. It is suitable for manual and mechanical operation.

Storage:

Store in a cool and dry place and use up as soon as possible after opening; If it cannot be used up at one time, it shall be sealed with nitrogen; The second opening needs to be used for defoaming, and the original storage period is six months.

packing:

20kg or 200kgiron drum


인기 탭: polyester t100 based casting polyurethane prepolymer, China, manufacturers, factory, buy